CONCENTRATION OF LATERITES USING BIOMAS

dc.contributor.authorMuriithi, Naftali
dc.contributor.authorNjoroge, Peter W.
dc.contributor.authorWachira, Jackosn
dc.contributor.authorWanjau, Ruth
dc.date.accessioned2026-11-09T11:00:50Z
dc.date.issued2013-06-12
dc.descriptionPatent Certificate
dc.description.abstractA method of concentrating iron in laterites to make the .rcn extraction process economical is disclosed. Concentration using biomass yields higher levels of iron by using appropriate ratio of biomass: laterites. The concentration of iron in the laterites was done by heating a laterite /charcoa! mixture in the temperature range 500-7000C in a ceramic container, a slow current of air (0.5-0.7em3/sec) was passed thus generating carbon monoxide in-situ. The process involves cooling and picking iron containing mineral. The optimum ratio of biomass: laterite was found to be 1 :20 by mass. The iron in the raw laterites is predominantly minerals goethite, FeO.OH and haematite, Fe203, as shown by presence of peaks at diffraction angles of 28 = 21.51 ° and 28 = 54.11 “respectively. After magnet-separation iron wes present predomisianily as the mineral, magnetite Fe304, with diffraction peak at 28 = 36°. The percentage of iron in the magnet-separated product is increased to 55-62%.
dc.description.sponsorshipKenyatta University Intellectual Property Rights Unit
dc.identifier.urihttps://repository.mut.ac.ke/handle/123456789/7179
dc.language.isoen
dc.publisherKenya Industrial Property Institute
dc.titleCONCENTRATION OF LATERITES USING BIOMAS
dc.typeOther

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Utility model Number 93.pdf
Size:
372.98 KB
Format:
Adobe Portable Document Format

License bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
2.05 KB
Format:
Item-specific license agreed upon to submission
Description:

Collections